Working condition
| Process | Hydrometallurgical Gold Extraction |
| Size | NPS6 (DN150) |
| Pressure Rating | CLASS 600 lb |
| Temperature | 225℃ |
| Acidic Slurry | Support |
| Material | TA10 (Grade 10 Titanium, UNS R52400) |
Pain Points and Proposal
1. Jamming, Internal Leakage, Short Service Life:
1.1 Seat coating corrosion/spalling
1.2 Seat sealing surface scratches
1.3 Spring corrosion failure
1.4 Solid buildup on ball
2. External Leakage:
1.1 Body flow path erosion
1.2 Body corrosion
Reference
CIS-R
Process: Hydrometallurgical gold extraction
Size: NPS 6
Pressure Rating: CLASS 600lb
Temperature: 260°C
Fluid: Mineral Slurry with Acid
Raw material: Ti10